Last Updated on November 17, 2026 by
Every piece of treated timber in your build has a job description printed on it. Most owner-builders never read it.
A fence post, a deck joist and a wall stud can all be sold as “treated pine” and all be completely wrong for where they’re going. The post that rots at ground level in four years and the joist that’s still sound in thirty were probably bought from the same yard, from the same stack, with the same green tinge.

The difference is the treatment class. Every country names it differently. This post covers why timber needs treating at all, what happens to untreated timber when you stress-test it above and below ground and how the Australian H classes, the American UC categories and the Canadian UC numbers map onto each other, so you can read a tag and know what you’re buying.
Why timber rots and why 20 per cent moisture is the line that matters
Wood decay isn’t old age. It’s digestion.
Decay fungi need four things to get going: food, which is the wood itself; oxygen; a mild temperature between about 10 and 35 degrees Celsius, with the optimum around 24 to 32; and moisture. Take away any one and the fungus stops.
You can’t take away the food or the oxygen. You can’t do much about the temperature either, so moisture is the only lever you control.
The moisture threshold is the useful part. Decay fungi need the wood to be above roughly 20 per cent moisture content and they do their best work once it passes the fibre saturation point, which sits around 28 to 30 per cent.
The USDA Forest Service’s Wood Handbook states it plainly: serious decay only occurs once moisture content is above fibre saturation. Below that line the wood is too dry to support the organism.
That single fact explains almost everything you’ll see on a building site. Roof framing in a 90 year old house is often untouched because it has never been wet.
A bearer 100 mm off the ground under a deck that can’t dry out is gone in a decade. Same timber, same species, different moisture.
Wood also gets eaten by things that don’t care about moisture content. Termites and borers take timber that’s perfectly dry. Marine borers do the same work in salt water.
That’s why the treatment classes name two hazards side by side, decay and insects. It’s also why a treatment that handles one may not handle the other.
What doesn’t kill timber: sunlight. Ultraviolet light breaks down lignin at the surface, which is why untreated boards go grey and hairy.
That’s cosmetic. Sapwood that greys can still be sound underneath. The structural failure, when it comes, is fungal or insect.
The stress test: what untreated timber actually does
Here’s the test that matters. You can run the logic on any block: put the same untreated pine in four places and watch what happens.
In the ground, untreated pine is gone fast. Australian Standard AS 5604 puts non-durable heartwood, which is what pine heartwood is, at zero to five years in ground contact where termites are active. Above ground and exposed to the weather, it’s zero to seven years.

Not decades. Years.
Field trials back this up. In USDA Forest Service post tests near San Juan, Puerto Rico, untreated posts averaged about 1.5 years in ground contact, ranging from 0.4 to 3.6 years depending on species.
Of 1,381 untreated posts in that work, only 3 per cent were still serviceable after 12 years. In cooler climates you get longer than that, but not the kind of longer that changes the decision.
Extension guidance from the University of Kentucky puts untreated pine posts at three to seven years and properly treated posts at 20 to 35.
Above ground and exposed, untreated timber does better but not well. The same AS 5604 figures give non-durable heartwood zero to seven years when it’s exposed to the weather and sheltered from termites.
The failure points are predictable. End grain sucks water in like a bundle of straws. Then come joints where water sits, the underside of a board that never sees sun, or any spot where soil, mulch or leaf litter stays in contact.
Above ground, dry and ventilated, untreated timber can last a century. Old barns and roof frames prove it. Shelter it from rain, let air move around it and keep it away from soil and it stops being a race.
In a wall cavity, untreated timber lasts the life of the house, which is why interior framing doesn’t need treatment in most of the world. In Australia it does. The reason is termites rather than rot.
Here’s the part that catches people. Rot starts inside. A post that looks sound shows a soft shell and a hollow centre when you press a screwdriver into it.
Brown rot fungi strip out the cellulose and leave a crumbly brown residue. The strength goes well before the surface tells you. By the time a deck joist looks bad it has usually been unsafe for years.

Sapwood, heartwood and the timbers that fight back on their own
A tree fights decay with chemistry it puts into the dead wood at its centre. That’s heartwood.
In a few species it’s durable in its own right. The living outer ring, the sapwood, is plumbing: porous, full of stored sugars and starch, which is food for anything with the right enzymes.
The commercial problem is that a pine board is mostly sapwood. So the sapwood has to be impregnated with something that kills fungi and insects. The process only works because sapwood is porous and takes the chemical in.
Heartwood does the opposite. The denser and more durable the species, the harder a preservative is to push into it.
This is why you can’t treat the heartwood of spotted gum or blackbutt to H4. It’s also why a treatment tag on a durable hardwood tells you very little. For those species you rely on natural durability or you change species.
The timbers that hold up on their own, heartwood only, include kwila (also sold as merbau) and teak in the tropics. In Australia there’s white cypress, tallowwood, spotted gum and the ironbarks.
In North America there’s western red cedar, white oak, black locust, osage orange and old growth redwood. They’re graded for it: AS 5604 puts Class 1 heartwood at 25 years plus in ground contact and 40 years plus above ground exposed, while Class 4 manages zero to five in the ground.
Two cautions. Durability ratings apply to the heartwood and say nothing about the sapwood on the same board, which will rot happily.
And decay resistance isn’t termite resistance. Some of the toughest hardwoods in the world are eaten by termites without complaint.
How a preservative actually gets into the wood
Treatment isn’t paint. It’s an industrial process with a specification.
The specification has two halves: how deep the chemical went and how much of it is in there. Penetration and retention. A product that fails either one doesn’t meet the standard, whatever the tag says.
The main processes:
- Vacuum pressure impregnation (VPI). Timber is sealed in a pressure vessel and put through cycles of vacuum and pressure. It’s how CCA, ACQ, copper azole and boron get deep into structural timber, decking and posts. This is the process behind almost everything rated for ground contact.
- Double vacuum, used with light organic solvent preservatives (LOSP). Applied to timber in its final shape, so joinery, fascia, balustrades and primed cladding. Out of ground contact only. It leaves the timber dry and dimensionally stable, which is why joinery suppliers like it.
- Diffusion, using boron. The green timber is treated wet and the preservative migrates through the water in the cells. It gives protection indoors against borers and termites but washes out, so it’s for flooring, furniture, mouldings and remedial work.
- Envelope treatment. The preservative penetrates 2 to 10 mm and the shell protects the core. Australia uses it for H2F framing and it works because the chemical both kills and repels termites.
- Glue-line treatment. Boron or a synthetic pyrethroid is added to the adhesive when plywood, LVL or particleboard is made. Insects only.
- Brush-on. Penetrates 3 mm at best. Maintenance and cut-end protection, nothing more.
Every one of these is only as good as the retention achieved. Any cut, notch, drill hole or rebate you make on site exposes untreated timber, which is why the standards all tell you to re-treat cut ends with two coats of a brush-on preservative at the time of construction, not later.
Three countries, three labels, one idea
Australia, the United States and Canada all answer the same question: how wet does this timber get and what’s trying to eat it? They just print the answer differently.
- Australia and New Zealand use AS/NZS 1604, which classifies by hazard class, H1 to H6. The number rises with the hazard.
- The United States uses AWPA Standard U1, which classifies by use category, UC1 to UC5, with letter subdivisions where the hazard needs finer tuning.
- Canada uses the CSA O80 series, also called use categories, but numbered UC1, UC2, UC3.1, UC3.2, UC4.1 and UC4.2.
The Canadian system looks like the American one at a glance and isn’t. UC3.2 in Canada is roughly UC3B in the United States.
UC4.1 is roughly UC4A. Confusing the two is easy and the labels don’t warn you.
The Australian hazard classes, H1 to H6
AS/NZS 1604 defines six hazard classes. The sets them out with their service conditions. Any product claiming to be preservative treated has to be branded with species, preservative, hazard class, standard reference and treatment plant.
- H1. Inside, above ground, protected from weather and termites. Borers only. Interior framing, flooring, furniture, joinery. It offers no protection against termites or decay.
- H2. Inside, above ground, protected from wetting, with termite risk. Borers and termites. The standard treatment for wall and floor framing across Australia. It assumes the timber stays dry, so it’s wrong for anything that gets wet.
- H2F. Inside, above ground, envelope treated. Termite protection with a treated shell rather than full penetration, used for framing south of the Tropic of Capricorn. Cheaper and acceptable in that application, but any cut through the envelope has to be re-treated.
- H3. Outside, above ground, periodic wetting and leaching. Moderate decay, borers and termites. The workhorse class: weatherboards, fascia, pergolas, decking, window and door joinery. Timber that gets wet and dries out again.
- H4. Outside, in ground, non-critical. Severe decay, borers and termites. Fence posts, landscaping timbers, pergola posts, retaining walls under one metre. This is the class most garden timber should be and often isn’t.
- H5. In ground or in fresh water, critical applications. Very severe decay, borers and termites. Structural retaining walls, piling, poles, house stumps, building poles.
- H6. Marine waters. Prolonged immersion in salt water, where marine borers are the threat as much as decay. Boat hulls, jetty piles, marine bracing and steps.
New Zealand splits several of these further, into H1.1, H1.2, H3.1 and H3.2. If you’re buying across the Tasman or reading a New Zealand supplier’s spec, H3.1 is a coated, non-structural product and H3.2 is the one rated for structural use and decking.
They aren’t interchangeable. The difference is one digit.
The H4 and H5 line is where most owner-builder money is wasted or saved. H4 is for non-critical work.
If the timber is holding up a structure or holding back more than a metre of soil, the standard answer is H5 or a Class 1 durable hardwood. AS 4678 gives residential retaining structures a 60 year design life, which isn’t a job for a treated post rated at the bottom of the in-ground range.
One more Australian point. A treatment class doesn’t replace a termite management system. AS 3660 covers that and treated framing is one layer of it, not the whole thing.
The American use categories, UC1 to UC5
The introduced the use category system in 1999. There are five biodeterioration categories plus one for fire retardants.
- UC1, interior dry. Protected from weather and from interior water sources. Furniture, millwork, interior construction.
- UC2, interior damp. Not in ground contact, protected from weather, but exposed to occasional moisture. Interior beams, flooring, framing, sill plates.
- UC3A, exterior above ground, protected. Either coated with rapid water runoff or fully protected by design from precipitation. Coated millwork, siding, trim.
- UC3B, exterior above ground, exposed. No coating required. Decking, railings, fence pickets, sills, walkways, deck joists.
- UC4A, ground contact, general use. Posts, structural lumber, deck joists and beams, freshwater docks, plus above-ground components that are critical or that may end up in ground contact.
- UC4B, ground contact, heavy duty. Severe environments, high decay climates, permanent wood foundations, building poles, utility poles, salt water splash zones.
- UC4C, ground contact, extreme duty. Very severe environments, land and freshwater piling, foundation piling, tropical poles.
- UC5A, UC5B and UC5C, marine. Split by region and by which marine borers are present, from northern waters through to the Gulf and Hawaii.
The part to memorise is the note under UC4A. It lists the above-ground situations that still have to be treated as ground contact: when soil, vegetation or leaf litter can build up against the timber, when construction or planting stops air circulating underneath, when a component sits less than six inches above final grade on a permeable support without a moisture break, when it touches untreated or already-decayed wood, when it gets wetted regularly, or when it’s in a tropical climate.
That note is why deck framing in the United States is routinely sold with a ground contact rating even though it never touches soil. It sits in the splash zone under the decking and the code assumes it will get wet.
The code itself spells out the triggers. IRC R317.1 requires naturally durable or preservative-treated wood in crawl spaces where joists are closer than 18 inches to exposed ground, girders closer than 12 inches and columns closer than 8 inches; for sills and sleepers on a slab in contact with the ground unless separated by a moisture barrier; for siding, sheathing and wall framing within 6 inches of the ground; for girder ends entering masonry with less than half an inch of clearance; for wood columns on basement slabs unless carried on piers or metal pedestals at least an inch above the floor; and for structural members supporting balconies, porches and similar appurtenances that are exposed to weather without a roof or overhang to keep water off the joints.
Reading a US tag is simple once you know what to look for. It carries the AWPA U1 reference, the use category, the preservative, the retention in pounds per cubic foot and the treating plant’s accreditation.
A tag reading “ACQ” on its own tells you nothing useful, because retention varies by category: for Southern pine, AWPA lists ACQ at 0.25 lb/ft³ for UC3B, 0.40 for UC4A and 0.60 for UC4B. Same chemical, three different products.
If a board has no legible tag, treat it as untreated. That’s the safe assumption and it costs you a few dollars of extra treatment rather than a deck.

The Canadian use categories and why the numbers move
Canada runs its own standard, the CSA O80 series. Its use category system is based on the AWPA one but renumbered to suit Canadian conditions and species.
- UC1. Interior, above ground, dry. Protected from moisture. Insects only.
- UC2. Interior, above ground, damp. Protected from weather but able to get damp. Decay fungi and insects.
- UC3.1. Exterior, above ground, coated with rapid water runoff. Decay fungi, staining fungi and insects. Coated millwork, siding, trim.
- UC3.2. Exterior, above ground, uncoated or poor runoff. Decking, deck joists, railings, fence pickets, uncoated millwork.
- UC4.1. Ground contact or fresh water, normal exposure, including salt water splash. Fence, deck and guardrail posts, bridge beams, crossties, building posts and poles in low decay areas.
- UC4.2. Ground contact or fresh water with high decay hazard, or critical components that are hard to replace. Piles, permanent wood foundations, building poles, horticultural posts, utility poles in high decay areas.
- UC5A. Coastal waters, brackish or salt, plus the adjacent mud zone. Piles, bulkheads, bracing.
Two Canadian details matter on site. Structural and ground contact lumber is incised before treatment, with rows of small cuts rolled into the faces, because spruce-pine-fir won’t take preservative deeply enough without it. The strength penalty is real and it’s built into the design standard, CSA O86, as a treatment factor.
The preservatives are also registered federally by Health Canada’s Pest Management Regulatory Agency. What’s on a Canadian shelf is what’s registered in Canada, which isn’t always the same list as the American one.
CCA is no longer available for residential construction in Canada, the same as in the United States. What you’ll find at a Canadian yard for decks and fences is ACQ or copper azole, usually in brown.
Translating between the three systems
For a rough conversion when you’re reading a foreign specification or buying imported timber:
- H1 is roughly UC1.
- H2 is roughly UC2, with termites added.
- H3 is roughly UC3B or UC3.2.
- H4 is roughly UC4A or UC4.1.
- H5 is roughly UC4B or UC4C, or UC4.2.
- H6 is roughly UC5A, UC5B or UC5C.
Treat those as approximate and no better. The hazard maps behind them differ, the species differ and the test methods differ.

Australia treats subterranean termites as a national default while the United States treats them as a regional problem, so an H2 rating carries a termite assumption that UC2 does not. If you’re building in Australia, buy to the Australian class. If you’re building in Texas, buy to the AWPA category.
Matching the treatment to the job
This is the table every owner-builder actually wants, in words rather than columns.
Decking boards. Above ground, regularly wetted and expected to look decent. H3 in Australia, UC3B in the United States, UC3.2 in Canada.
In Australia the APVMA’s label rules stop CCA-treated timber being supplied for domestic decking, so ask for ACQ or copper azole rather than assuming the green board is fine for a surface your kids crawl on. If you want to skip preservatives altogether, is the other option and it pays to work out the rather than just the boards.
Deck joists and bearers. These live in the splash zone under the decking, which is the wettest part of the structure and the part nobody sees. In the United States they’re treated as ground contact, so UC4A.
In Australia, H3 is acceptable where the sub-floor is well ventilated and the bearer sits 400 mm or more above the ground. Below that, H4. Canadian deck joists are normally UC3.2, with UC4.1 where the design puts them low.
Deck posts. In the ground, so H4 minimum in Australia and H5 if they’re structural, UC4A or UC4B in the United States, UC4.1 or UC4.2 in Canada.
Better still, keep the post out of the soil on a galvanised post base or a concrete pier with a capillary break. A treated post that never touches soil lasts far longer than the class requires.

Fence posts. H4 in Australia, UC4A in the United States, UC4.1 in Canada. This is the classic false economy: an H3 or above-ground post buried in soil fails at the ground line, which is the one part you can’t inspect without digging.
Retaining walls. Under a metre and not structural, H4 is the conventional Australian answer. Over a metre, or anything engineered, H5 or a Class 1 hardwood.
In North America, UC4B or UC4.2 for anything critical. Check the local code as well, because retaining walls above a certain height usually need engineering.
Pergola and carport posts. If they go into the ground, treat them as posts. If they sit on brackets above a slab, H3, UC3B or UC3.2 is enough.
Cladding and fascia. H3 in Australia and LOSP-treated primed fascia is common because it holds its shape and takes paint. UC3A or UC3B in the United States, UC3.1 or UC3.2 in Canada. These boards get wet on one face and dry on the other, so paint maintenance is part of the protection.
Landscaping timber and garden sleepers. H4 minimum. Never in contact with soil you’re growing food in.
Interior framing. H2 in Australia for termite protection and it’s only one layer of it: is a system, not a board. UC2 in the United States, where borate treatments are common indoors.
In Canada, UC2 applies where the framing can get damp. If you’re still choosing between materials, the comparison covers the rest of the decision.
Marine. H6, or UC5A to UC5C, or UC5A in Canada. Nothing else.
Salt water borers will open untreated or under-treated piles like a tin can. There’s no maintenance schedule that saves them.
Planters, compost bins and anything holding soil. This is the highest hazard in a domestic garden, because the timber is permanently wet and permanently in contact with soil. H4 is a floor, not a target.
Health Canada advises against treated wood in compost bins, mulch or edging for an edible garden. Build those from untreated durable hardwood, or line them.
The chemicals and what changed since 2003
CCA, chromated copper arsenate. The green timber that built a generation of decks and playgrounds. Copper and arsenic do the work, chromium fixes them in the wood. It’s effective, cheap and extremely well proven in ground contact and marine use.
What changed is where it’s allowed. In 2003 the manufacturers withdrew CCA from residential use in the United States. Canada followed.
Australia’s APVMA completed a review in 2005 and changed the labels: CCA-treated timber can’t be supplied for garden furniture, picnic tables, exterior seating, children’s play equipment, patio and domestic decking, or handrails. It remains a mainstay for poles, piling, marine timbers and industrial work.
ACQ, copper azole and micronised copper azole. Copper-based with no arsenic. The default residential product in North America.
They work. They’re also more corrosive to fasteners than CCA and they leach copper at the surface, so the fastener rules matter: hot dip galvanised to ASTM A153, or stainless steel. Don’t mix stainless fasteners into galvanised connectors, or the two metals will eat each other.
Boron. Excellent against borers and termites indoors and useless outdoors because it washes out. Interior framing, flooring, furniture.
LOSP. Tebuconazole and propiconazole for fungi plus a synthetic pyrethroid for insects, carried in a light solvent. That’s the Australian answer for primed joinery, fascia and cladding. It’s unsuitable for ground contact.
Creosote and pentachlorophenol. Industrial preservatives for poles, crossties, piling and marine work. They work, they smell and you don’t want them in a residential application or on anything a child touches.
Handling, all of them. Cut and machine treated timber outdoors, wear a dust mask and gloves, wash before eating, don’t burn offcuts in a fire pit or a wood heater, don’t use treated timber for cutting boards, mulch, animal bedding or edible garden edging. Dispose of offcuts through your local waste system rather than the backyard burn.
The mistakes that kill treated timber
- Cutting the ends and walking away. Every cut through treated timber exposes untreated timber at the most absorbent part of the board. Two coats of brush-on copper naphthenate at the time of construction, not at the end of the job.
- Notching and boring after treatment. Same problem, bigger hole.
- Buying above-ground treatment for in-ground work. An H3 or UC3B post in soil fails at the ground line within a few years. It’s the single most common treatment error on a DIY site.
- Burying offcuts as packers. Untreated packers, formwork offcuts and spacers left under a bearer or inside a wall can’t dry and rot, then take the treated timber around them with them.
- No airflow under a deck. Joists 100 mm off the ground with no cross ventilation stay damp permanently. Ground clearance and airflow are part of the treatment.
- Letting soil or mulch build up against timber. Splash-back and soil contact turn an above-ground member into a ground contact member, whatever the tag says.
- Storing timber flat on the ground on site. Weeks of sitting in wet grass is enough to start staining fungi and, in sapwood, decay.
- Mismatched fasteners and flashing. Galvanised nails in ACQ timber corrode faster than the timber rots. Stainless fasteners against galvanised connectors create a galvanic cell. Match the metals to the treatment and to each other.
- Sealing a wet board. Coating timber above about 20 per cent moisture traps the water in. Check it before you paint it.
- Assuming “treated” means “won’t rot”. Treatment buys time in one hazard class. It doesn’t make pine into teak.
Questions we get asked
How long will treated timber last? It depends on the class and the detailing, which is why the range is wider than most people expect. Full penetration H4 and H5 softwood posts in Australian in-ground service are modelled at more than 100 years in the worst decay zone and around 35 to 80 years in milder zones, while an H3 post in the same soil will be gone inside a decade. Above ground and protected from rain, almost any treated timber will outlive the person who built with it.
Can I use treated timber for raised garden beds? Not with copper or arsenic treatments if you’re growing food in it. Health Canada advises against treated wood in compost bins, mulch or edible garden edging.
Australian label rules block CCA for garden furniture and similar frequent-contact uses. Untreated durable hardwood, or a lined bed, is the straightforward answer.
Is it safe to burn treated timber offcuts? No. Burning releases the preservative in the smoke and ash, which is why every regulator in the three countries bans it. Bag it and send it to landfill or a transfer station.
My board says UC4A. Can I use it above ground? Yes. Higher categories meet the requirements of lower ones. What you can’t do is the reverse: a UC3B deck board isn’t a UC4A post, however similar it looks.
Why isn’t H4 always enough in Australia? Because H4 is defined as non-critical. If the member is structural, or holding back more than a metre of soil, or expensive to replace, the requirement moves to H5 or a Class 1 hardwood. The class describes the hazard, not the importance of the job, so importance gets added on top.
Does painting treated timber make it last longer? It helps, but it’s second-order. Paint slows the wetting and drying cycle and stops surface checking, which extends service life, but it can’t rescue timber that’s in the wrong hazard class.
The tag is the contract
Treatment class is one of the few things on a building site you can verify in ten seconds with your phone torch and no tools. Read the end tag before the timber goes on the ute.
Match the class to where the timber’s going, not where it’s sold. Then seal every cut.
Do that and treated pine does what it’s sold to do. Skip it and you’ll be rebuilding the same deck in eight years, wondering why the boards looked fine right up until the day they didn’t.
If you’re pricing the job now, before you choose the boards. If you’re building into the cooler months, changes the cost as much as the class does.
Want more? Subscribe to our weekly newsletter!
Sources
- (hazard classes H1 to H6, treatment methods, preservative types)
- (AS 1604 hazard classes, sapwood treatability, fixings)
- (AS 5604 durability classes, in-ground service life model, retaining wall design life)
- (2005 label restrictions on CCA)
- (UC1 to UC5 definitions, UC4A note 1)
- (use category list, retention table for Southern pine)
- (CCA)
- (untreated post service life, Puerto Rico)
- (CSA O80 use categories, incising, fasteners, field treatment)
- (untreated pine post life)